doing a commercial 2/3 day job at the mo,glass panels are six foot wide by 20 foot high......
bout 50 glass panels , at the side junction between each glass panel there is a border. bout 10mm maybe which is made up of silicone a rubber seal i make it. Prob is im getting slight spotting along the side junction between each panel....
my process of cleaning has been to cleab each 20 x 6 panel one at time ie. scrub, rince on glass , rince off
no spotting anywhere else just in these places
opinions lads
cheers and thanks in advance
no pics but its the same as many commercial jobs and im sure some of u guys have solution

im thinking i just need rince 5/6 panels together at one time , then no splashbacks when i move onto next panel??!